 IEC 60794-4: Stress-strain test for ADSS, Breaking strength test for ADSS, Creep test for ADSS
IEC 60794-4: Stress-strain test for ADSS, Breaking strength test for ADSS, Creep test for ADSS
IEEE 1138:Creep test for OPGW, stress-strain test for OPGW, Ultimate tensile strength test for OPGW, Twist test of OPGW (custom made)
IEC 61395:Creep test for stranded conductors
BS EN 50182, IEC 61089:Stress-strain test for stranded conductors
ASTM B524: Tensile test for conductors
IEC 61232: Tensile test, Elongation test, Stress at 1% extension
IEC 61284: Mechanical failure testing for fittings

IEEE 1138:Creep test for OPGW, stress-strain test for OPGW, Ultimate tensile strength test for OPGW, Twist test of OPGW (custom made)
IEC 61395:Creep test for stranded conductors